250° Cure Prepreg Carbon Fiber Fabric 2×2 Twill 6k 50″/127cm 11oz/372gsm Hyosung H2550 C10

SKU: G-374-50-202D-38-M-C-D

$97.76

    Add to Compare
    Categories: ,

    Please Note: Due to the nature of composite materials, coloration of fabric may change or darken when resin is introduced to your part/fabric.

    Description

    CE 4092 is a modified epoxy pre-impregnated system which can cure at 250°F (121°C) for one hour. CE 4092 can be supplied on any commercially available glass, Kevlar, or graphite fabric. Both sides of the fabric are pre-impregnated yielding a double sided tack material with the CE 4092 prepreg system. CE 4092 prepreg system can be used for laminating and honeycomb sandwich construction.

    This prepreg fabric has a width of 50″, tow size of 6k and is woven in a 2×2 twill weave. This material is woven tighter than most of our competitors’ fabrics. This will help ensure a straight weave and a better looking final product.

    Sold by the linear yard with a 5 yard minimum purchase required.

    Cure Cycle

    CE 4092 can be cured at 250°F (121°C) for one hour, however shorter cures are possible at higher temperatures.

    The prepreg may be cured using either standard heat-up methods or by in-hot, out-hot press applications. A pressure of 30 psi is recommended, however pressures of 10 to 50 psi may be used.

    Storage & Out Life

    Store material in a contaminate free container and store at 0 degrees F for extended storage. For shorter storage time requirements store at 40 degrees F, this enables quicker stabilization times.

    MECHANICAL PROPERTIES
    Based upon 0.125 inch thick cured laminate consisting of CE 4092 on 7781 glass cloth cured at 250°F (121°C) for one hour.
    Mechanical Property Test Method Test Condition Test Values
    Tensile Strength ASTM D 638 @ 75°F dry 63,400 psi
    Tensile Modulus ASTM D 638 @ 75°F dry 3.5 X 106 psi
    Compressive Strength ASTM D 695 @ 75°F dry 48,600 psi
    Flexural Strength ASTM D 790 @ 75°F dry 80,100 psi
    Flexural Modulus ASTM D 790 @ 75°F dry 3.0 X 106 psi
    Interlaminar Shear Strength ASTM D 2344 @ 75°F dry 7,450 psi

    Application

    Remove material from cold storage at least 20 hours prior to use to allow for stabilization at room temperature. Keep the material wrapped to prevent moisture from condensing on the adhesive. If details are cut and replaced into cold storage, shorter stabilization times may be used.

    Cut the prepreg to size, remove the poly separator and apply to part or mold. Remove separator paper. Continue process until the desired number of plies are obtained. Debulking is recommended after every 5 – 20 plies. The material may be debulked at temperatures up to 120°F. When lay-up is complete, the prepreg can be cured in a vacuum bag in an oven or autoclave. Apply at least 10 psi pressure and cure for one hour at 250°F.

    Health and Safety

    This material contains epoxy resins and amines which may cause irritation to sensitive skin. Avoid contact with eyes or skin. If contact with skin occurs, wash as soon as possible with soap and water. If contact with eyes occurs, flush with water for 15 minutes. Do not handle or use this material until Material Safety Data Sheet has been read and understood. The user of this material is required to use the necessary protective equipment as directed by applicable state and federal laws when handling, curing, and grinding this material.

    Shipping: This material should be shipped expedited airmail. Due to a short shelf life at room temp we suggest shipping this material via an expedited service such as UPS Overnight, 2-day or 3-day. These are guaranteed services. If these are chosen, we will ship the materials in the beginning of the week to ensure they do not sit in the shipping company warehouse over the weekend. We send the material with insulation and icepacks. It is suggested that you ship with 2-day airmail at a minimum. If you plan to use material within days of arrival or are OK with loosing days of shelf life, you can select any shipping method you would like, however if our minimum suggested shipping method is not chosen, we will not be held responsible for issues with material.

    Custom Prepreg Options

    We can have almost any of our fabrics pre-impregnated for you. Please email us for more details. We have systems in our PREG3xx series that can cure at various temps from 86° F to 275° F with safe service temps of over 600° F. We can do a max width of 60″ and also offer toughened systems. Lead times are usually 2-3 weeks for custom prepreg. We can do single side or double sided prepreg, vary the resin % in the cloth and vary the tack level of the material. Options are endless.

    We take care in shipping our items and we will never fold the fabric. Our fabric is always rolled onto a tube to prevent distortion of the weave.

    0/5 (0 Reviews)

    Additional information

    Unit of Measure

    Shipping

    Resin Content

    Volatile Content

    Separator

    Shelf Life

    Material Warp

    Material Weft

    Weave

    Ends Per Inch

    Pics Per Inch

    Yarn Size Warp

    Yarn Size Weft

    Tow Size

    Weight

    Width

    Thickness

    CE4092 TDS

    CE4092 SDS

    Reviews

    There are no reviews yet.

    Only logged in customers who have purchased this product may leave a review.

    How We Sell - Fabrics

    Our fabrics are sold by the linear yard, with the exception of our samples which are a single 4"x4" (or 5"x7") piece. The unit price displayed is for 1 linear yard; all volume discounts will be automatically applied when selecting larger quantities of fabric when added to your shopping cart, as indicated in the table above with quantity discount ranges for units purchased.

    Please purchase the number of linear yards that you require. When purchasing multiple yards of the same fabric, you will receive one continuous length of that material. We carefully take that material and roll it onto a cardboard core and wrap clear plastic or Kraft paper over it, making sure to keep the fabric in its first quality condition. We pride ourselves on having one of the best material handling crews possible.

    Resin Consumption

    Resin consumption is provided for the approximate amount of resin by weight in the final part after processing by vacuum infusion. This does not account for the resin used in the flow lines and consumables such as flow media or breather cloth. Wet-layup by hand will also have a higher resin consumption in the final part and depends on the user’s techniques. Vacuum bagging a wet layup will improve the resin content. Too much resin will cause a weaker part, not stronger. The average rule of thumb is around 45% (+/- a couple of percent). To calculate actual resin % in your part, a burn test is used. For example, you have a part weighing 100 grams, and you would burn off the resin, which would leave the fiber behind. You should have 55 grams of fiber left when your process is working correctly. Due to the variables in processing, it is hard to give an accurate amount of resin needed to purchase for making your part. However, you will have waste no matter what method is used. A suggested ratio is about 1-1.5lbs of resin per lb of fabric purchased.

    Compare Products